Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 8700X Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Opaque Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 1010 A Natural Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Izod Impact, Notched | 10.0 J/cm @Temperature 23.0 °C |
18.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Europe-Africa-Middle East) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched | 10.0 J/cm @Temperature 23.0 °C |
18.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Notched | 10.0 J/cm @Temperature -20.0 °C |
18.7 ft-lb/in @Temperature -4.00 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP KUR 1010 TG05 Polypropylene, 5% Mineral Filled PP copolymer 5% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 10.0 J/cm @Temperature 23.0 °C |
18.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |