Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -17.8 °C |
13.0 ft-lb/in @Temperature 0.000 °F |
ASTM D256 |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -17.8 °C |
13.0 ft-lb/in @Temperature 0.000 °F |
ASTM D256 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-BU00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 12.7 mm |
13.0 ft-lb/in @Thickness 0.500 in |
LW, E-48/50 |
Industrial Laminates/Norplex MC514MG Glass Fabric Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
13.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 5220 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.96 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.96 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® S1500 High Heat PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
13.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers DIAMALOY PC 1113 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
13.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall SP-6655 Rigid PVC, Molding Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |