Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
10.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 5.80 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched | 5.80 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched | 5.80 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched | 5.82 J/cm @Temperature 23.0 °C |
10.9 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1651 + PPE blend (10/90) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |