Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.360 J/cm @Temperature -40.0 °C |
0.674 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -40.0 °C |
0.674 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar EN052 Polyester Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature -40.0 °C |
0.674 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Izod Impact, Notched | 0.360 J/cm @Temperature 23.0 °C |
0.674 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |