Polymer Property : Izod Impact, Notched = 0.356 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.190 J/cm

@Temperature 23.0 °C
0.356 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® INP630 ABS
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
Izod Impact, Notched 0.190 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
0.356 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Izod Impact, Notched 0.190 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
0.356 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec..
Izod Impact, Notched 0.190 J/cm

@Temperature -20.0 °C
0.356 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Prisma 3410 is a medium melt flow rate random copolymer designed for injection molding. This product exhibits exceptional transparency, very good stiffness/impact strength balance, and excellent pro..
Izod Impact, Notched 0.190 J/cm

@Temperature -20.0 °C
0.356 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem RP 344 RACO Random Polypropylene Copolymer
RP 344 is a medium melt flow rate random copolymer. It is suitable for blown and cast film extrusion and features good processability, excellent optical properties, and outstanding sealability. Its ..