Polymer Property : Izod Impact, Notched = 1.39 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.39 J/cm

@Thickness 6.35 mm
2.60 ft-lb/in

@Thickness 0.250 in
ASTM D256
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 1.39 J/cm

@Temperature -30.0 °C
2.60 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® IR2840 PC
7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit..
Izod Impact, Notched 1.39 J/cm

@Temperature -30.0 °C
2.60 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXRL0662 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
Izod Impact, Notched 1.39 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.60 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Ineos ABS Lustran® ABS 241 ABS, Blending Grade
Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Izod Impact, Notched 1.39 J/cm

@Temperature 23.0 °C
2.60 ft-lb/in

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Ineos L70Z-01 Polypropylene Impact Copolymer
L70Z-01 is a nucleated and antistatic high flow polypropylene medium impact copolymer for injection molding applications. This product meets the requirements of the U.S. Food and Drug Administration..
Izod Impact, Notched 1.39 J/cm

@Temperature -20.0 °C
2.60 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Ineos N00G-01 Polypropylene Impact Copolymer
Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa..
Izod Impact, Notched 1.39 J/cm

@Temperature -20.0 °C
2.60 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
Ineos N20N-00 Polypropylene Impact Copolymer
This is a high melt flow rate, nucleated polypropylene impact copolymer formulated for improved flowability. It has an optimum balance of stiffness and impact resistance for injection molded applic..
Izod Impact, Notched 1.39 J/cm

@Temperature -40.0 °C
2.60 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade
Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W..
Izod Impact, Notched 1.39 J/cm

@Temperature -30.0 °C
2.60 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene
Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination ..
Izod Impact, Notched 1.39 J/cm

@Thickness 6.35 mm,
Temperature -40.0 °C
2.60 ft-lb/in

@Thickness 0.250 in,
Temperature -40.0 °F
ASTM D-256
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 1.39 J/cm

@Thickness 6.35 mm,
Temperature -40.0 °C
2.60 ft-lb/in

@Thickness 0.250 in,
Temperature -40.0 °F
ASTM D-256
Axiall 7803 Rigid PVC, Extrusion High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 1.39 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.60 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Axiall 9209 Rigid PVC, Molding
Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati..