Polymer Property : Izod Impact, Notched = 0.637 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.637 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.19 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Izod Impact, Notched 0.637 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.19 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Izod Impact, Notched 0.637 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.19 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMIPLAS LD590 Light diffusion ABS
Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical
Izod Impact, Notched 0.637 J/cm

@Thickness 6.35 mm
1.19 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.637 J/cm

@Thickness 6.35 mm
1.19 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® GR-4030 ABS, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.637 J/cm

@Temperature -20.0 °C
1.19 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H5211PBR High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Non pressure pipes, co-extruded pipes as the inner layerInformation provided by SCG Chemicals
Izod Impact, Notched 0.637 J/cm

@Temperature 23.0 °C
1.19 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P851JO Polypropylene Injection Molding
Key Characteristics:Good processabilityHigh gloss and brightnessOdorlessSafe for food contactRecommended Applications:Clear food containerClear large size containerThin wall productsInformation prov..