Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.392 J/cm @Temperature -20.0 °C |
0.735 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP640S Injection Molding Grade Polypropylene Moplen EP640S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640S is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.50 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.256 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HI5204S PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HI5205 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.50 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.256 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HF5150H PP+MF15%, High Flow Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature 23.0 °C |
0.735 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys.. |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature -20.0 °C |
0.735 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature 0.000 °C |
0.735 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part.. |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature 0.000 °C |
0.735 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P851JO Polypropylene Injection Molding Key Characteristics:Good processabilityHigh gloss and brightnessOdorlessSafe for food contactRecommended Applications:Clear food containerClear large size containerThin wall productsInformation prov.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm |
0.735 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm |
0.735 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |