Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.374 J/cm @Temperature -20.0 °C |
0.700 ft-lb/in @Temperature -4.00 °F |
1/8" (3mm) notched bar; ASTM D256 |
Ineos N01N-00 Polypropylene Impact Copolymer Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti.. |
|||
Izod Impact, Notched | 0.374 J/cm @Temperature -18.0 °C |
0.700 ft-lb/in @Temperature -0.400 °F |
ASTM D256 |
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6335N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
0.701 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
0.701 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Diamond Polymers NPP 60-1010 PCTA Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.374 J/cm @Temperature 0.000 °C |
0.701 ft-lb/in @Temperature 32.0 °F |
ASTM D256A |
Dow C705-44NA Polypropylene Impact Copolymer Resin DOW C705-44NA Polypropylene Resin is a high melt flow rate impact copolymer that combines superior stiffness and good impact resistance. The product is intended for use in injection molding applica.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
0.700 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall CL-6380, CL-6380J Rigid PVC, Molding Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where vis.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
0.700 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
0.700 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall NR-5009 Rigid PVC, Molding Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, .. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
0.700 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall SP-6340 Rigid PVC, Molding Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited .. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
0.700 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall MD-5009 Rigid PVC, Molding Georgia Gulf MD-5009 is a rigid, fitting-grade PVC compound designed for hot spruce/runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, whi.. |
|||
Izod Impact, Notched | 0.374 J/cm @Temperature -30.0 °C |
0.700 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.Former A-Top Polymers product; part of Amco product line since 2013.. |