| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 103 | 103 | ASTM D785 |
| Tensile Strength at Break | 51.0 MPa | 7400 psi | ASTM D638 |
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
| Elongation at Break | 300 % | 300 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
| Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
| Izod Impact, Notched | 0.374 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
0.701 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
| 0.800 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 | |
| Impact Test | 42.0 J @Temperature 23.0 °C |
31.0 ft-lb @Temperature 73.4 °F |
High speed instrumented impact (puncture); Energy @ max load; ASTM D3763 |
| 48.0 J @Temperature -40.0 °C |
35.4 ft-lb @Temperature -40.0 °F |
High speed instrumented impact (puncture); Energy @ max load; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | 0.125";; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 149 °C | 300 °F | 0.125";; ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 0.30 % | 0.30 % | ASTM D1003 |
| Transmission, Visible | 89 % | 89 % | ASTM D1003 |
| 91 % | 91 % | Total transmission; ASTM D1003 |