Mechanical Properties Metric English Comments
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
PolyMirae Moplen EP640T Injection Molding Grade Polypropylene
Moplen EP640T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640T is a block copolymer suitable for injection molding of a..
Izod Impact, Notched 0.294 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
0.551 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HIPS MI730 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Izod Impact, Notched 0.294 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
0.551 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Izod Impact, Notched 0.294 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
0.551 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Izod Impact, Notched 0.294 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
0.551 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Izod Impact, Notched 0.294 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
0.551 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Izod Impact, Notched >= 0.294 J/cm

@Thickness 6.40 mm,
Temperature -10.0 °C
>= 0.551 ft-lb/in

@Thickness 0.252 in,
Temperature 14.0 °F
ASTM D256
LG Chemical LUPOL GP3200 PP+MF20%
Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched >= 0.294 J/cm

@Thickness 6.40 mm,
Temperature -10.0 °C
>= 0.551 ft-lb/in

@Thickness 0.252 in,
Temperature 14.0 °F
ASTM D256
LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness
Description: Injection Molding, PP+MF20%, Good Weatherability, High StiffnessApplication: Automotive Interior Parts CAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Izod Impact, Notched 0.294 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.551 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.294 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.551 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.294 J/cm

@Temperature 23.0 °C
0.551 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P700J Polypropylene Injection Molding
Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa..
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding
Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t..
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part..
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric..
Izod Impact, Notched 0.294 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
0.551 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Izod Impact, Notched 0.294 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.551 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.294 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.551 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled
Information provided by Samsung Cheil Industries.