PolyMirae Moplen EP640T Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP640T Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Moplen EP640T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640T is a block copolymer suitable for injection molding of automotive parts, parts of electrical appliances and housewares, etc. Features: Optimized balance of stiffness and toughness; High impact strength even at low temperature; Narrow molecular weight distribution; Low warpageApplications: TWIM; AutomotivesInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 51 g/10 min

@Load 2.16 kg,
Temperature 230 °C
51 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 27.5 MPa
3980 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.67 GPa
242 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.686 J/cm

@Temperature 23.0 °C
1.29 ft-lb/in

@Temperature 73.4 °F
ASTM D256