Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 56.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 76.0 J
56.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP COLORCOMP D10006U PC
LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed.
Impact Test 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXRL0682 PC Copolymer
18 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Impact Test 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli..
Impact Test 76.0 J
56.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Impact Test 76.0 J
56.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved