Polymer Property : Impact Test = 40.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 54.2 J

@Temperature 22.8 °C
40.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R6000 FR-PC Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Impact Test 54.2 J
40.0 ft-lb
Schmolz + Bickenbach MoldMAX® SC Copper Alloy
Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot ..
Impact Test 54.2 J

@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa..
Impact Test 54.2 J

@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa..
Impact Test 54.2 J

@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa..
Impact Test 54.2 J

@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa..
Impact Test 54.2 J

@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa..
Impact Test 54.2 J
40.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Impact Test 54.2 J
40.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Impact Test 54.2 J

@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
DescriptionPolyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency. NOTE: Physical properties are based on rotationa..