Mechanical Properties Metric English Comments
Impact Test 29.0 J

@Temperature -29.0 °C
21.4 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax 7823 Polypropylene Impact Copolymer, Fractional Melt Flow
Key Features: high extrudate melt strength, good cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: pipe, tubing, sheet, profiles, netting, blown containers and i..
Impact Test 29.0 J

@Temperature -29.0 °C
21.4 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax SB786 Polypropylene Impact Copolymer
Key Features: blush-resistant, easy molding, high impact polypropylene copolymer resin, good cold impact resistance, good stiffness, FDA acceptableApplications: automotive battery case, housewares, ..
Impact Test 29.0 J
21.4 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Impact Test 29.0 J
21.4 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Impact Test 29.0 J
21.4 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS
LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque.
Impact Test 29.0 J

@Thickness 4.00 mm
21.4 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix
AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polybutylene Terephthalate (PBT) resin matrix. This composite material fea..
Impact Test 29.0 J

@Temperature -30.0 °C
21.4 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
LyondellBasell Hifax™ ETA-3131 Thermoplastic Olefin Resin
Key Features: medium melt flow, medium modulus thermoplastic olefin resin, excellent impact and stiffness balance, excellent processabilityApplications: automotive filler and valance panels, lower a..