Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 18.1 J | 13.3 ft-lb | Direct; Gardner |
Lord Adhesives Aeroglaze® 9924 Wash Primer Aeroglaze® 9924 wash primer was designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.All information provided by .. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Reverse; Gardner |
Lord Adhesives Aeroglaze® 9924 Wash Primer Aeroglaze® 9924 wash primer was designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.All information provided by .. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Direct; Gardner |
Lord Adhesives Aeroglaze® 9924V Wash Primer Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided b.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Reverse; Gardner |
Lord Adhesives Aeroglaze® 9924V Wash Primer Aeroglaze® 9924V wash primer was designed for priming metal surfaces. It is particularly useful for priming non-ferrous substrates such as aluminum and galvanized steel.All information provided b.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Direct; Gardner |
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Reverse; Gardner |
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Forward/reverse |
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and c.. |
|||
Impact Test | >= 18.1 J | >= 13.3 ft-lb | |
Abatron AboThane 8003-3 Polyurethane Coating AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, .. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moistu.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | 0.32 cm x 7.6 cm x 7.6 cm, 1.6 cm diameter tup; ASTM G14 |
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating Scotchkote Fusion Bonded Epoxy coating 206N XTRA LG is one-part, heat curable, thermosetting, powdered epoxy coating with extended gel for coating the interior of line pipe and fittings, valves, and.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Forward and Reverse |
Blue River Coatings CRC100-H BLUE RIVER COATINGS CRC100-H is a two-component inorganic corrosion resistant coating designed for Original Equipment Manufacturers (OEM) to protect metal substrates from corrosion and abrasion. If .. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | 12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester |
3M Scotchcast™ 265 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | 0.32cm x 7.6cm x 7.6cm steel panel, 1.6cm radius tup; ASTM G14 |
3M Scotchkote™ 412 Fusion Bonded Epoxy Coating 3M Scotchkote Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to preheated steel.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | 0.32cm x 7.6cm x 7.6cm steel panel, 1.6cm radius tup; ASTM G14 |
3M Scotchkote™ 412 Spray Grade Fusion Bonded Epoxy Coating 3M Scotchkote Spray Grade Fusion Bonded Epoxy Coating 413 is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of reinforcing steel. The epoxy is applied to pre.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Direct; Gardner |
Lord Adhesives Aeroglaze® A276 Reflective Polyurethane Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.All information provi.. |
|||
Impact Test | 18.1 J | 13.3 ft-lb | Reverse; Gardner |
Lord Adhesives Aeroglaze® A276 Reflective Polyurethane Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.All information provi.. |