Impact Test 1.80 J
1.33 ft-lb
Multi-Axial Instrumented Impact Energy; ISO 6603-2
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev..
Impact Test 1.80 J
1.33 ft-lb
puncture strength; ASTM D5748
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade
Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri..
Impact Test 1.80 J
1.33 ft-lb
ASTM D256
3M Scotchkote™ PR 415 Epoxy Concrete Repair
Scotchkote Epoxy Concrete Repair PR 415 has been specifically developed as a three component 100% solids self priming concrete repair system.Product Features:Combines good application characteristic..
Impact Test 1.80 J
1.33 ft-lb
ASTM D256
3M Scotchkote™ 474 Epoxy Concrete Repair
Scotchkote Epoxy Concrete Repair 474 has been specifically developed as a three component 100% solids high performance mortar for use as a heavy duty repair system for concrete surfaces.Product Feat..
Impact Test 1.80 J
1.33 ft-lb
Spencer Impact ASTM D3420
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 125 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..