Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0250 GPa | 3.63 ksi | ISO 37 |
Huntsman AVALON® 95 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | DIN 53504 |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | DIN 53504 |
Huntsman IROGRAN® A 98 P 4535 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou.. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil.. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-A895 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ASTM D412 |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ISO 37 |
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
300% Modulus | 0.0250 GPa | 3.63 ksi | ISO 37 |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |