Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0270 GPa | 3.92 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0270 GPa | 3.92 ksi | ISO 37 |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
300% Modulus | 0.0270 GPa | 3.91 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0270 GPa | 3.92 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0270 GPa | 3.92 ksi | ASTM D412 |
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
300% Modulus | 0.0270 GPa | 3.92 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0270 GPa | 3.91 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 40 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0270 GPa | 3.92 ksi | ASTM D412 |
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |