Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plastolein 9057 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa @Temperature 145 °C, Time 2990 sec |
1.86 ksi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 6250 High Acrylonitrile Polymer Description: NBR 6250 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6250 is a non staining, medium mooney, an.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Plastolein 9057 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 15 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 5 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0128 GPa | 1.86 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P General Purpose Molding FormulationNordel® IP 4725P |
|||
300% Modulus | 0.0128 GPa | 1.86 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9060 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 78A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |