Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0103 GPa | 1.49 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0103 GPa | 1.50 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | Vulcanized |
KKPC KOSYN 1712G Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | Vulcanized |
KKPC KOSYN 1724 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0103 GPa @Temperature 145 °C, Time 2100 sec |
1.49 ksi @Temperature 293 °F, Time 0.583 hour |
ASTM D412 |
LG Chemical SBR 1712 High Acrylonitrile Polymer Description: SBR 1712 is an oil extended cold polymerization SBR with 37.5 parts of highly aromatic oil and styrene-butadiene copolymer of 23.5% bound styrene. Raw materials for this product are ca.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0103 GPa | 1.50 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 |
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
300% Modulus | 0.0103 GPa | 1.50 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 ASTM D3568 FormulationNordel® IP 5565 |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |
|||
300% Modulus | 0.0103 GPa | 1.50 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
300% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412-98 |
Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight toleranc.. |