Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00241 GPa | 0.350 ksi | |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
300% Modulus | 0.00241 GPa | 0.350 ksi | Machine Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412 |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
300% Modulus | 0.00241 GPa | 0.350 ksi | Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® G1657 M (SEBS) Linear Block Copolymer Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id.. |
|||
300% Modulus | 0.00241 GPa | 0.350 ksi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® G1657 M (SEBS) Linear Triblock Copolymer Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id.. |
|||
300% Modulus | 0.00241 GPa | 0.350 ksi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® D1116 K (SBS) Radial Triblock Copolymer Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified.. |
|||
300% Modulus | 0.00241 GPa @Time 7200 sec |
0.350 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-9 TPE Product Description: StarTUFF TF 75-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
300% Modulus | 0.00241 GPa | 0.350 ksi | ASTM D 412 |
CPT C-Flex® R70-085 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |