Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D412 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ISO 37 |
Kraton® D4271 J (O/E SBS) Branched Block Copolymer Description: Kraton D4271 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene of 45% mass. It is supplied from Japan in the physical forms identified in .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 400501S SBS Based Material, 50A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 402501S SBS Based Material, 50A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 500500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600300S SEBS Based Material, Filled Qualities, 30A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600350S SEBS Based Material, Filled Qualities, 35A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 602350S SEBS Based Material, Filled Qualities, 35A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 602400S SEBS Based Material, Filled Qualities, 40A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 602450S SEBS Based Material, Filled Qualities, 45A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 602500S SEBS Based Material, Filled Qualities, 50A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 662500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
300% Modulus | 0.00200 GPa | 0.290 ksi | ASTM D638 |
ELASTO UK Dryflex® 600500S SEBS Based Material, Filled Qualities, 50A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |