Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6906 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6907 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6201 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6202 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6205 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6206 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6209 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6210 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6211 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6301 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6302 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6305 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6308 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6309 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6310 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6902 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | steel/steel |
Resinlab® AR 4315 Metal Bonding Methacrylate Adhesive Resinlab™ AR 4315 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6203 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6204 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6207 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6208 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6304 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6306 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6307 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6901 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | SSPC SP3-Dry; ASTM D1002 |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6903 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6904 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6905 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Adhesive Bond Strength | 29.0 MPa | 4200 psi | Steel lap shear |
Resinlab® CYNERGY CA6908 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |