Mechanical Properties Metric English Comments
Adhesive Bond Strength 2.76 MPa

@Temperature 23.9 °C
400 psi

@Temperature 75.0 °F
Maple to itself at 50% R.H. Test at 0.1 inches/min. separation rate.
3M Scotch-Grip™/Fastbond™ 5298 Industrial Adhesive  (discontinued **)
An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.One part, 100% solids moisture curing liquid urethane adhesive which ca..
Adhesive Bond Strength 2.76 MPa
400 psi
Grit blasted steel
Loctite® 417 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Excellent - 100% Concrete
Chesterton ARC 791 Composite
Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex..
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
concrete; ASTM D4541
Chesterton ARC 797 Low-viscosity, 100% solids, epoxy-based, concrete primer sealer
Description: Its unique hydrophobic properties allow ARC 797 to be applied to damp concrete with excellent penetrating properties. When applied, ARC 797 will improve adhesion of subsequent topcoats ..
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Excellent - 100% Concrete
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Dry Concrete; ASTM D4541
Chesterton ARC PW Potable Water Coating
Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea
EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea
EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea
EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea
EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL..
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer
EP 3001, “Powered by Reactamine® Technology”, is a two component 100% solid polyurea based sealant. EP 3001 is a self-leveling sealant designed to protect horizontal concrete. This elastomer disp..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone
EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi..
Adhesive Bond Strength 2.76 MPa
400 psi
Al-to-Al Lap Shear; Cured property;5 mil bondline thickness on primed aluminum panels; ASTM D1002
Aptek 2712-A/B Very low stress silicone adhesive
Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad..
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP JS EPI Engineered Polymers Joint Sealant
EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP RP EPI Engineered Polymers Aromatic Polyurea
EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC EP RSP EPI Engineered Polymers Silicone Polyurea
EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti..
Adhesive Bond Strength 2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea
ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst..