Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | >= 10.0 MPa | >= 1450 psi | Phenolic, Substrate Failure, Shear; ISO 4587 |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Zinc, Shear; ISO 4587 |
Permabond 2010 Cyanoacrylate, gap filling PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Adhesive Bond Strength | >= 10.0 MPa | >= 1450 psi | Phenolic, Substrate Failure, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Zinc, Shear; ISO 4587 |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Zinc, Shear; ISO 4587 |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Adhesive Bond Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | Grit blasted mild steel, Shear; ISO 4587 |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Adhesive Bond Strength | 10.0 - 20.0 MPa | 1450 - 2900 psi | steel collar and pin shear; ISO 10123 |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | steel collar and pin shear; ISO 10123 |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Adhesive Bond Strength | 10.0 - 11.0 MPa | 1450 - 1600 psi | Glass/steel, Shear |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Zinc, Shear; ISO 4587 |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Zinc, Shear; ISO 4587 |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Adhesive Bond Strength | 10.0 - 12.0 MPa | 1450 - 1740 psi | Carbon Fiber, Shear; ASTM D1002 |
Permabond ES569 Epoxy Resin PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | steel collar and pin shear; ISO 10123 |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | steel collar and pin shear; ISO 10123 |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Lap Shear Cohesive Strength; ASTM D1002 |
ITW Plexus Plexusâ„¢ AO420FS Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies. |
|||
Adhesive Bond Strength | >= 10.0 MPa | >= 1450 psi | on Alumina substrate |
Gwent Electronic Materials C2050830D8 80:20 Silver Palladium Ink C2050830D8 is an ink based on a 80:20 ratio of Silver:Palladium. It is designed for use in Single Layer PZT applications. This ink can be used in both dip and hand soldering. This Ink is in a ready .. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | Tensile shear per ASTM D1002 on etched Al panel |
Von Roll Isola IMI E-Solder® 3017 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Adhesive Bond Strength | 10.0 MPa @Temperature -54.4 °C |
1450 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-34 Epoxy Adhesive This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste.. |
|||
Adhesive Bond Strength | 10.0 MPa | 1450 psi | steel collar and pin shear; ISO 10123 |
Permabond MH052 Anaerobic Threadsealant Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1.. |
|||
Adhesive Bond Strength | 10.0 - 20.0 MPa | 1450 - 2900 psi | steel collar and pin shear; ISO 10123 |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |