Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel lap shear |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel lap shear |
Resinlab® CYNERGY CA6702 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel lap shear |
Resinlab® CYNERGY CA6701 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 854-1 Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 4 hrs @ 65°C |
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive TRA-BOND F202 is a clear, low viscosity epoxy adhesive recommended for photonic applications requiring exposure to high temperatures or chemical and environmental resistance. This 100% solids system.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Varies with substrates |
Loctite® 312 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, cured 8 hrs |
Tra-Con Tra-Bond 2202 Low Viscosity/High Temperature Epoxy Adhesive TRA-BOND 2202 is a low viscosity, high temperature cure epoxy resin system developed for rigid laminating, filament winding, potting and bonding applications where a clear, almost transparent adhesi.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | |
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | |
Trelleborg Emerson & Cuming Eccobond® A 359 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming A 359 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveAluminum filled, heat curing, epoxy adhesive. Sag resistant. Exceptional thermal and chemical resistance. H.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Grit blasted steel |
Loctite® 426 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel/Steel; Varies with substrates |
Loctite® 609 General Purpose Retaining Compound Retainers: Loctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel/Steel; Varies with substrates |
Loctite® 640 Medium Strength/High Temperature Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Steel/Steel; Varies with substrates |
Loctite® 675 Medium Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Adhesive Bond Strength | 20.7 - 41.4 MPa | 3000 - 6000 psi | Varies with substrates |
Loctite® Durabond® E-120HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | >= 20.7 MPa | >= 3000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-106 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Adhesive Bond Strength | >= 20.7 MPa | >= 3000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-130M-1 Unfilled Epoxy Adhesive A two-component, non-hazmat, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Adhesive Bond Strength | >= 20.7 MPa | >= 3000 psi | Lap Shear Strength |
Epoxyset Epoxibond EB-135 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-135 has excellent bond strength to various substrat.. |
|||
Adhesive Bond Strength | 20.7 MPa @Temperature -54.4 °C |
3000 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-7/W Epoxy Adhesive, 3:2 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 931-1T1N1 Thixotropic Epoxy Encapsulant TRA-BOND 931-1T1N1 epoxy encapsulant is designed for good adhesion, providing strong resilient bonds to a wide variety of substances. This is a thixotropic version of TRA-BOND 931-1.Information prov.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear, alum to alum, 2 hrs @ 70°C |
Tra-Con Tra-Bond 970-1N1 General Purpose Epoxy Adhesive TRA-BOND 970-1N1 is a general purpose epoxy that exhibits sag resistance and excellent bond strength to a wide variety of substrates. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Adhesive Bond Strength | 20.7 - 34.5 MPa | 3000 - 5000 psi | Varies with substrates |
Loctite® Durabond® E-20HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Adhesive Bond Strength | 20.7 MPa | 3000 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Adhesive Bond Strength | 20.7 - 34.5 MPa | 3000 - 5000 psi | Varies with substrates |