Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 2.76 MPa @Temperature 23.9 °C |
400 psi @Temperature 75.0 °F |
Maple to itself at 50% R.H. Test at 0.1 inches/min. separation rate. |
3M Scotch-Grip™/Fastbond™ 5298 Industrial Adhesive
(discontinued **) An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.One part, 100% solids moisture curing liquid urethane adhesive which ca.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Grit blasted steel |
Loctite® 417 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | >= 2.76 MPa | >= 400 psi | Excellent - 100% Concrete |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |
|||
Adhesive Bond Strength | >= 2.76 MPa | >= 400 psi | concrete; ASTM D4541 |
Chesterton ARC 797 Low-viscosity, 100% solids, epoxy-based, concrete primer sealer Description: Its unique hydrophobic properties allow ARC 797 to be applied to damp concrete with excellent penetrating properties. When applied, ARC 797 will improve adhesion of subsequent topcoats .. |
|||
Adhesive Bond Strength | >= 2.76 MPa | >= 400 psi | Excellent - 100% Concrete |
Chesterton ARC 988 Composite Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi.. |
|||
Adhesive Bond Strength | >= 2.76 MPa | >= 400 psi | Dry Concrete; ASTM D4541 |
Chesterton ARC PW Potable Water Coating Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
Adhesive Bond Strength | >= 2.76 MPa | >= 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer EP 3001, “Powered by Reactamine® Technology”, is a two component 100% solid polyurea based sealant. EP 3001 is a self-leveling sealant designed to protect horizontal concrete. This elastomer disp.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Al-to-Al Lap Shear; Cured property;5 mil bondline thickness on primed aluminum panels; ASTM D1002 |
Aptek 2712-A/B Very low stress silicone adhesive Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad.. |
|||
Adhesive Bond Strength | >= 2.76 MPa | >= 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP JS EPI Engineered Polymers Joint Sealant EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP RP EPI Engineered Polymers Aromatic Polyurea EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti.. |
|||
Adhesive Bond Strength | 2.76 MPa | 400 psi | Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer |
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst.. |