Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349K Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349K epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349K is excellent for bonding many metals and woods, most plastics.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349M Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349M epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349M is excellent for bonding many metals and woods, most plastics.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum, 2 hrs @ 65°C |
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy TRA-DUCT 925M01 is a low ion snap cure silver-filled epoxy. TRA-DUCT 925M01 develops strong, durable, void free electrically and thermally conducting bonds. The product can be screen printed, stenci.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 9349 Room Temperature Cure Flexible Epoxy Adhesive TRA-BOND 9349 epoxy adhesive is a flexible, two part, room temperature curing system with high peel and sheer strengths. TRA-BOND 9349 is excellent for bonding many metals and woods, most plastics a.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond Ablebond 481-20 B-Stageable Epoxy Adhesive Ablebond 481-20 flexible epoxy adhesive is a modification of Ablebond 481-19 adhesive. This adhesive is designed to absorb stresses between adherends with mismatched coefficients of thermal expansio.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | Grit blasted steel |
Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | 10.3 MPa @Temperature -54.4 °C |
1500 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-2/H20 Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Adhesive Bond Strength | 10.3 MPa @Temperature 25.0 °C |
1500 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-271 Epoxy Adhesive A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled .. |
|||
Adhesive Bond Strength | 10.3 MPa @Temperature 82.2 °C |
1500 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong X-81-A/F Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP QSZ EPI Engineered Polymers Quick Set Epoxy with Zinc EP QSZ Quick Set Epoxy with Zinc, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s (Volatile Organic Compound), self-leveling modified epoxy. This versatile new gene.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC is, aliphatic polyurea (silicone optional) coating, that was developed for UV stable (col.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP 60 EPI Engineered Polymers Aliphatic Polyurea EP RAP 60 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, coating (silicone optional) developed for UV stable (colorfast) polyurea flooring applic.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (no primer), Substrate Failure; ASTM D4541 Elcometer |
ACC EP RP EPI Engineered Polymers Aromatic Polyurea EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time.. |
|||
Adhesive Bond Strength | 10.3 MPa | 1500 psi | cured |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Adhesive Bond Strength | >= 10.3 MPa | >= 1500 psi | Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer |
ACC EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea f.. |