Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.179 GPa | 26.0 ksi | ASTM D790 |
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
2% Secant Modulus | 0.179 GPa | 26.0 ksi | ASTM D790 |
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
2% Secant Modulus | 0.179 GPa | 26.0 ksi | Crosshead Speed - 1/2 in/min; ASTM D790 |
LyondellBasell Petrothene® NA860008 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
2% Secant Modulus | 0.179 GPa | 26.0 ksi | Crosshead Speed - 1/2 in/min; ASTM D790 |
LyondellBasell Petrothene® NA860241 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |