Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Typical |
Industeel FORA 500 500 HB Wear Resistant Steel Description: FORA 500 is a water quenched martensitic steel, with a 500HB (51.5 HRC), typical hardness, resistant to very severe abrasion wear. Thanks to its mechanical properties, good toughness, h.. |
|||
Charpy Impact | 30.0 J | 22.1 ft-lb | |
Haynes 230® alloy, plate, 4000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Charpy Impact | 30.0 - 50.0 J @Temperature -17.8 °C |
22.1 - 36.9 ft-lb @Temperature 0.000 °F |
|
Latrobe CBS-50™ NiL VIM-VAR High Performance Carburizing Bearing and Gear Steel CBS-50 NiL VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case .. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
|
ThyssenKrupp XAR® 400 Structural Steel This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 400.Application: The steel may be used for wear exposed structures, e.g. excavati.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
|
ThyssenKrupp XAR® 450 Structural Steel This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 450.Application: The steel may be used for wear exposed structures, e.g. excavati.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
|
ThyssenKrupp XAR® PLUS Structural Steel This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® PLUS.Application: The steel may be used for wear exposed structures, e.g. excavat.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp SECURE 200 Structural Steel This Material Specification applies to heavy plates from 3 to 15 mm in thickness made of the high-strength armour steel SECURE 200 (ThyssenKrupp armour steel) with a minimum hardness of 200 HBW and .. |
|||
Charpy Impact | 30.0 J | 22.1 ft-lb | Hardening Temperature- 1120°C; Tempering Temperature- 550°C |
Crucible Steel CPM® 10V® (AISI A11) Tool Steel CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan.. |
|||
Charpy Impact | 30.0 J | 22.1 ft-lb | V-notch |
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |