Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 12.0 MPa @# of Cycles 1.00e+8 , Temperature 140 °C |
1740 psi @# of Cycles 1.00e+8 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Fatigue Strength | 12.0 MPa @# of Cycles 1.00e+8 , Temperature 140 °C |
1740 psi @# of Cycles 1.00e+8 , Temperature 284 °F |
R = 0.1, 8 Hz, dry |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Fatigue Strength | 12.0 MPa @# of Cycles 10000 , Temperature 180 °C |
1740 psi @# of Cycles 10000 , Temperature 356 °F |
|
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |