Modulus of Elasticity 2.41 - 4.50 GPa
350 - 653 ksi
Average value: 3.73 GPa Grade Count:7
Overview of materials for Thermoplastic Polyimide, Unfilled
Modulus of Elasticity 4.10 - 4.50 GPa

@Temperature 60.0 - 150 °C
595 - 653 ksi

@Temperature 140 - 302 °F
Average value: 4.33 GPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Modulus of Elasticity 0.0250 - 4.50 GPa
3.63 - 653 ksi
Average value: 1.69 GPa Grade Count:45
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..