Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.20 - 3.50 GPa | 464 - 508 ksi | ASTM D638-04 |
Proto3000 Objet RGD525 High Temperature Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Modulus of Elasticity | 2.25 - 3.50 GPa | 327 - 508 ksi | Average value: 3.02 GPa Grade Count:53 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 0.900 - 3.50 GPa | 131 - 508 ksi | Average value: 1.83 GPa Grade Count:35 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 0.400 - 3.50 GPa @Temperature 40.0 - 150 °C |
58.0 - 508 ksi @Temperature 104 - 302 °F |
Average value: 1.37 GPa Grade Count:5 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 3.00 - 3.50 GPa | 435 - 508 ksi | |
Hybrid Plastics POSS® EP 1000 Epoxy Adhesive EP1000 is a POSS® based epoxy adhesive with outstanding oxidative resistance to ozone, plasma, or atomic oxygen environments. The EP1000 POSS® Epoxy is also well-suited for peroxide and steam... |
|||
Modulus of Elasticity | 3.00 - 3.50 GPa | 435 - 508 ksi | |
Hybrid Plastics POSS® EP 1050 Epoxy Adhesive EP1050 is a POSS® based, high-temperature epoxy adhesive with outstanding resistance to ozone, plasma, or atomic oxygen environments. Major applications include medical devices, optics, semicondu.. |
|||
Modulus of Elasticity | 0.350 - 3.50 GPa | 50.8 - 508 ksi | Average value: 1.45 GPa Grade Count:44 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Modulus of Elasticity | 1.30 - 3.50 GPa | 189 - 508 ksi | Average value: 2.72 GPa Grade Count:5 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Modulus of Elasticity | 0.750 - 3.50 GPa | 109 - 508 ksi | Average value: 1.35 GPa Grade Count:43 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |