Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 14.0 - 17.0 GPa | 2030 - 2470 ksi | Injection; ISO 527 |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Modulus of Elasticity | 1.60 - 17.0 GPa | 232 - 2470 ksi | Average value: 3.03 GPa Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Modulus of Elasticity | 1.10 - 17.0 GPa @Temperature 60.0 - 175 °C |
160 - 2470 ksi @Temperature 140 - 347 °F |
Average value: 10.4 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Modulus of Elasticity | 4.00 - 17.0 GPa | 580 - 2470 ksi | Average value: 9.55 GPa Grade Count:8 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Modulus of Elasticity | 3.40 - 17.0 GPa | 493 - 2470 ksi | Average value: 8.25 GPa Grade Count:10 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Modulus of Elasticity | 3.90 - 17.0 GPa | 566 - 2470 ksi | Average value: 9.07 GPa Grade Count:100 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Modulus of Elasticity | 6.90 - 17.0 GPa | 1000 - 2470 ksi | Average value: 12.9 GPa Grade Count:18 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |