Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 0.600 GPa | >= 87.0 ksi | ISO.178 DN.53452 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Modulus of Elasticity | 0.600 - 12.1 GPa | 87.0 - 1750 ksi | Average value: 2.43 GPa Grade Count:36 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | 0.600 - 8.31 GPa @Temperature -40.0 - 150 °C |
87.0 - 1210 ksi @Temperature -40.0 - 302 °F |
Average value: 3.50 GPa Grade Count:5 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Modulus of Elasticity | 0.600 - 12.1 GPa | 87.0 - 1750 ksi | Average value: 6.84 GPa Grade Count:104 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Modulus of Elasticity | 0.600 - 41.4 GPa | 87.0 - 6000 ksi | Average value: 2.65 GPa Grade Count:125 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Modulus of Elasticity | 0.600 GPa | 87.0 ksi | ISO R527 |
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Modulus of Elasticity | 0.600 GPa | 87.0 ksi | Conditioned; ISO 178 |
Addiplast Addinyl A2 X Nylon 66 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | 0.600 GPa | 87.0 ksi | Conditioned; ISO 178 |
Addiplast Addinyl C2 R Nylon 66/6 High impact resistanceInformation provided by Addiplast. |
|||
Modulus of Elasticity | >= 0.600 GPa | >= 87.0 ksi | ISO.178 DN.53452 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Modulus of Elasticity | 0.600 - 15.4 GPa @Temperature 60.0 - 175 °C |
87.0 - 2230 ksi @Temperature 140 - 347 °F |
Average value: 4.73 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |