Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.30 - 11.0 GPa | 769 - 1600 ksi | Average value: 6.79 GPa Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Modulus of Elasticity | 5.30 - 140 GPa @Temperature -55.0 - 177 °C |
769 - 20300 ksi @Temperature -67.0 - 351 °F |
Average value: 86.9 GPa Grade Count:18 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Modulus of Elasticity | 5.30 GPa | 769 ksi | ISO 527 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Modulus of Elasticity | 5.30 GPa | 769 ksi | ISO 527-1/-2 |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Modulus of Elasticity | 5.30 - 8.40 GPa @Temperature 60.0 - 90.0 °C |
769 - 1220 ksi @Temperature 140 - 194 °F |
Average value: 7.70 GPa Grade Count:12 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |