Polymer Property : Modulus of Elasticity = 609 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.20 GPa
609 ksi
1 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
Modulus of Elasticity 4.20 - 8.20 GPa
609 - 1190 ksi
Average value: 5.46 GPa Grade Count:5
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 4.20 GPa
609 ksi
Lehmann & Voss LUVOCOM® 1105-7741 PEEK, with mineral filler, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Modulus of Elasticity 4.20 GPa
609 ksi
Toyobo ECOVYLOPET® EMC2311 PET Bottle Recycling Grade, 10% Glass Reinforced
Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo..
Modulus of Elasticity 4.20 GPa
609 ksi
After flexural test; ASTM D790, DIN EN ISO 178
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al..
Modulus of Elasticity 4.20 GPa
609 ksi
Conditioned; ISO 178
Addiplast Addilene H 490 M40F Flame Retardant Polypropylene, 40% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.