Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.45 GPa
500 ksi
ASTM D638
Technetics Group Amicon™ PEEK  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Modulus of Elasticity 3.45 - 11.0 GPa
500 - 1600 ksi
Average value: 6.46 GPa Grade Count:25
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Modulus of Elasticity 3.45 - 11.7 GPa
500 - 1700 ksi
Average value: 7.36 GPa Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M45 Polyester Film, 50 Gauge (15 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45..
Modulus of Elasticity 3.45 - 15.5 GPa
500 - 2250 ksi
Average value: 8.61 GPa Grade Count:108
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 3.45 - 32.4 GPa
500 - 4710 ksi
Average value: 16.1 GPa Grade Count:64
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Modulus of Elasticity 3.45 GPa
500 ksi
ISO 527
GEHR Plastics PA 6.6 Nylon 6.6, Dry
Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be ..
Modulus of Elasticity 3.45 GPa
500 ksi
ISO 527-2
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M33 Polyester Film, 50 Gauge, PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. the coating is heat sealable, and is an excellent moisture and..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M34 Polyester Film, 50 Gauge (13 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® MC2 Polyester Film, 50 Gauge (14 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A polyester film with a vacuum deposited layer of aluminum on one side and overcoated on both sides with a heat sealable PVDC copolymer. The film has exce..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Modulus of Elasticity 3.45 GPa
500 ksi
(stiffness), ASTM D882
DuPont Teijin Films Mylar® M45 Polyester Film, 75 Gauge (22 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45..
Modulus of Elasticity 3.45 - 3.79 GPa
500 - 550 ksi
Average value: 3.55 GPa Grade Count:10
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum an..
Modulus of Elasticity 3.45 - 5.86 GPa
500 - 850 ksi
Average value: 4.51 GPa Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..