Polymer Property : Modulus of Elasticity = 479 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638
Plaskolite Optix® CA-924 Impact Modified Acrylic Resin
Injection Molding Grade Pellets. Good impact strength.
Modulus of Elasticity 3.30 GPa
479 ksi
dry
Murtfeldt Murylon® B Nylon 6
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope..
Modulus of Elasticity 3.30 GPa
479 ksi
dry
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
Modulus of Elasticity 3.30 GPa
479 ksi
50% RH
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638
Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin
Injection Molding Grade Pellets. Good impact strength.
Modulus of Elasticity 3.30 GPa
479 ksi
ISO 527
Polycasa Lumina CAST PMMA
QUINN CAST lumina has even transmission of light across the whole surface when the sheet is illuminated through its edges. QUINN CAST lumina allows a reduction in final frame dimensions. Perfect for..
Modulus of Elasticity 3.30 - 20.3 GPa
479 - 2940 ksi
Average value: 6.89 GPa Grade Count:65
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Modulus of Elasticity 3.30 GPa
479 ksi
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Modulus of Elasticity 3.30 GPa
479 ksi
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Modulus of Elasticity 3.30 GPa
479 ksi
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Modulus of Elasticity 3.30 GPa
479 ksi
ISO 527
GEHR Plastics PMMA Acrylic
Polymethylmethacrylate is refractory and shows a good mechanical strength, tensile strength and hardness. PMMA is also scratch resistant and easy to polish. It shows good temperature resistance and ..
Modulus of Elasticity 3.30 GPa

@Temperature 25.0 °C
479 ksi

@Temperature 77.0 °F
Storage
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive
LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po..
Modulus of Elasticity 3.30 GPa
479 ksi
ISO 178
Addiplast Addinyl B2 1 Flame Retardant Nylon 6
Flame retardant, halogen freeInformation provided by Addiplast.
Modulus of Elasticity 3.30 GPa
479 ksi
GB/T 1040
Beijing Evergrow Resources Enylon®
Information provided by Beijing Evergrow Resources.
Modulus of Elasticity 3.30 GPa
479 ksi
dry
Murtfeldt Murylat® SP Polyethylene Terephthalate
Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri..
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638
Toyobo T-751 Nylon, Painting Grade
Key Feature: Glass fiber and mineral reinforced, high heat distortion and impact gradesInformation provided by Toyobo Co., Ltd
Modulus of Elasticity 3.30 - 6.30 GPa

@Temperature 60.0 - 120 °C
479 - 914 ksi

@Temperature 140 - 248 °F
Average value: 5.17 GPa Grade Count:2
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638; DIN 53452
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent  (discontinued **)
Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009.
Modulus of Elasticity 3.30 - 3.40 GPa

@Temperature 80.0 - 80.0 °C
479 - 493 ksi

@Temperature 176 - 176 °F
Average value: 3.37 GPa Grade Count:3
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Modulus of Elasticity 3.30 - 11.0 GPa

@Temperature -40.0 - 100 °C
479 - 1600 ksi

@Temperature -40.0 - 212 °F
Average value: 5.19 GPa Grade Count:27
Overview of materials for Polypropylene with 30% Glass Fiber Filler