Mechanical Properties Metric English Comments
Modulus of Elasticity 3.172 GPa
460.1 ksi
ASTM D638
Ineos Nova 1280 High Heat Crystal Polystyrene  (discontinued **)
Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r..
Modulus of Elasticity 3.172 GPa
460.1 ksi
ASTM D638
Ineos Nova 2110 General Purpose Crystal Polystyrene  (discontinued **)
Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure..
Modulus of Elasticity 3.172 GPa
460.1 ksi
Abatron AboCast 8-13/Abocure 8-13 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 53 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°..
Modulus of Elasticity 3.172 GPa
460.1 ksi
Abatron AboCast 8-18/Abocure 8-18 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c..
Modulus of Elasticity 3.172 GPa
460.1 ksi
ASTM D638
Ineos Nova 1290 High Heat Crystal Polystyrene
Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r..
Modulus of Elasticity 3.172 GPa
460.1 ksi
Lucite International XL Sanitary Ware Acrylic Sheet
Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an..
Modulus of Elasticity 3.172 GPa
460.1 ksi
ASTM D638
Ineos Nova 1200 High Heat Crystal Polystyrene
Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia..
Modulus of Elasticity 3.172 GPa
460.1 ksi
ASTM D638
Ineos Nova 1204 High Heat Crystal Polystyrene