Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 248 GPa | 36000 ksi | |
Kennametal Stellite Stellite® 21 Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti.. |
|||
Modulus of Elasticity | 248 GPa | 36000 ksi | In Tension |
Cytec Thornel® T-650/35 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Modulus of Elasticity | 248 GPa | 36000 ksi | |
CMW® THERMKON® 65M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Modulus of Elasticity | 248 GPa | 36000 ksi | |
CMW® THERMKON® 68 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Modulus of Elasticity | 248 GPa | 36000 ksi | (hardened and tempered) |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |