Mechanical Properties Metric English Comments
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa
30900 ksi
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, cold rolled sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Modulus of Elasticity 213 GPa
30900 ksi
Latrobe Lescalloy® Jethete M-152 ESR 2.25" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Modulus of Elasticity 213 GPa
30900 ksi
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Modulus of Elasticity 213 GPa
30900 ksi
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â..
Modulus of Elasticity 213 GPa
30900 ksi
ThyssenKrupp XABO® 355 Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Modulus of Elasticity 213 GPa
30900 ksi
ThyssenKrupp XABO® 500 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Modulus of Elasticity 213 GPa
30900 ksi
ThyssenKrupp XABO® 355 T Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Modulus of Elasticity 213 GPa
30900 ksi
ThyssenKrupp XABO® 500 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Modulus of Elasticity 213 GPa

@Temperature 300 °C
30900 ksi

@Temperature 572 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..
Modulus of Elasticity 213 GPa

@Temperature 100 °C
30900 ksi

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..
Modulus of Elasticity 213 GPa
30900 ksi
ThyssenKrupp XABO® 460 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Modulus of Elasticity 213 GPa
30900 ksi
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel
LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°..