Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 100 °C |
28100 ksi @Temperature 212 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Modulus of Elasticity | 194 GPa | 28100 ksi | Calculated |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Modulus of Elasticity | 194 GPa | 28100 ksi | |
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Modulus of Elasticity | 194 GPa @Temperature 316 °C |
28100 ksi @Temperature 601 °F |
plate heat treated to 1177°C and rapid quenched |
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |