Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Pacific Sintered Materials FX-227-T Infiltrated Steel Powdered Metal Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1005-50All information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Pacific Sintered Materials FX-232-T Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-50All information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Pacific Sintered Materials FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-110HTAll information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
PCC-Advanced Forming Technology 30% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Schott N-LAF36 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical; Solution treated |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Wieland Porta Maximum NF PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | Bar, Rod & Forgings |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | Castings & Strip |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Alliance S-26A Samarium Cobalt Magnetic Material |
|||
Modulus of Elasticity | 110 GPa @Temperature 1200 °C |
16000 ksi @Temperature 2190 °F |
|
ATI Wah Chang Nb/Nb Alloy FS-85 Information provided by ATI Wah Chang |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Alliance S-22A Samarium Cobalt Magnetic Material |
|||
Modulus of Elasticity | 110 GPa | 16000 ksi | |
Alliance S-22B Samarium Cobalt Magnetic Material |