Mechanical Properties Metric English Comments
Modulus of Elasticity 10.5 - 11.2 GPa
1520 - 1620 ksi
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Isoflow Graphite Rings facilitate an even flow of oil around the circumference of the billet. This even flow results in improved billet surface quality over long casting campaigns. Isoflow Graphit..
Modulus of Elasticity 10.5 GPa
1520 ksi
Poco Graphite AXM-5Q Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Modulus of Elasticity 10.5 - 16.5 GPa
1520 - 2400 ksi
Average value: 12.8 GPa Grade Count:11
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Modulus of Elasticity 10.5 GPa
1520 ksi
Lehmann & Voss LUVOCOM® 1/CF/15/TF/20/BK Polyamide 66, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
Modulus of Elasticity 10.5 GPa
1520 ksi
ASTM D638-10
DSM Somos® PerFORM Stereolithography Polymer, UV Postcure
PerFORM produces strong, stiff, high-temperature resistant composite parts on standard 355 nm stereolithography machines. This material’s lower viscosity makes processing parts faster. It exhibits ..
Modulus of Elasticity 10.5 GPa
1520 ksi
ISO 178
Addiplast Addinyl A2 V40 Nylon 66, 40% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 10.5 GPa
1520 ksi
ISO 178
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 10.5 GPa
1520 ksi
ISO 527-2
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable..
Modulus of Elasticity 10.5 GPa
1520 ksi
Poco Graphite TM Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Modulus of Elasticity 10.5 GPa
1520 ksi
ISO 527-2
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..