Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 12.4 - 28.0 GPa | 1800 - 4060 ksi | Average value: 21.5 GPa Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Modulus of Elasticity | 1.10 - 28.0 GPa | 160 - 4060 ksi | Average value: 7.84 GPa Grade Count:105 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Modulus of Elasticity | 10.3 - 28.0 GPa | 1500 - 4060 ksi | Average value: 20.3 GPa Grade Count:39 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |