Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0111 - 2.76 GPa
1.61 - 400 ksi
Average value: 1.23 GPa Grade Count:13
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 2.21 - 2.76 GPa
320 - 400 ksi
Average value: 2.46 GPa Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Modulus of Elasticity 0.000300 - 2.76 GPa
0.0435 - 400 ksi
Average value: 0.256 GPa Grade Count:64
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..