Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 100A CP Titanium Industry Specifications: USA Aerospace: AMS 4921. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specifications BS TA. 7, 8, 9.Features: The mechanical prope.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: .. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries .. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265 Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Aged Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to aged material; other specific condition entries are also available in MatWeb.Features: Cold formable and we.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2) Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical; Solution treated |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A .. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w.. |
|||
Modulus of Elasticity | 105 - 120 GPa | 15200 - 17400 ksi | Typical |
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Titanium Alloy Medium-Strength Surgical Implant AlloyFeatures: TIMETAL 367 is a dedicated, medium strength, titanium alloy for surgical implants. The alloy was developed specifically for the manufacture of femora.. |
|||
Modulus of Elasticity | 110 - 120 GPa | 16000 - 17400 ksi | Typical |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |