Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.765 - 12.4 GPa | 111 - 1800 ksi | Average value: 8.36 GPa Grade Count:47 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Modulus of Elasticity | 2.90 - 12.4 GPa | 420 - 1790 ksi | Average value: 8.85 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Modulus of Elasticity | 5.52 - 12.4 GPa | 800 - 1800 ksi | Average value: 9.72 GPa Grade Count:16 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Modulus of Elasticity | 1.10 - 12.4 GPa | 160 - 1800 ksi | Average value: 3.02 GPa Grade Count:64 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 8.27 - 12.4 GPa | 1200 - 1800 ksi | Average value: 10.2 GPa Grade Count:4 |
Overview of materials for Nylon 11 with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ.. |
|||
Modulus of Elasticity | 5.50 - 12.4 GPa | 798 - 1800 ksi | Average value: 10.4 GPa Grade Count:21 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Modulus of Elasticity | 3.79 - 12.4 GPa | 550 - 1800 ksi | Average value: 7.63 GPa Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 3.59 - 12.4 GPa | 520 - 1800 ksi | Average value: 8.31 GPa Grade Count:76 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |